DTG print looks fuzzy with fibres poking through: 3 things every new DTG owner must know
Short answer: Fibres poking through a DTG print come from how the shirt is handled after pretreatment. Fix it with 3 habits: press light at 175–180°C for 50–60 seconds with the lowest pressure, the Teflon sheet must not stick (it should lift off by itself, no pulling), and do not touch the print area (move the shirt by its corners).
Your DTG print comes out fuzzy, with tiny fibres poking up through the ink. This is one of the most common problems for shops with their first DTG printer, and it usually has nothing to do with the printer or the ink. It comes from pressing the pretreatment and handling the shirt before printing. Watch SK's short video (Thai), then read the 3 steps below.
🎬 Video summary (Thai) · 82 seconds
What fibres poking through look like

Cotton has tiny fibres on its surface. When they lie flat, the white ink covers the shirt smoothly. When they stand up before printing, they poke through the ink layer and the print looks fuzzy. It shows most on dark shirts.
Fibres get lifted at 3 moments: while pressing, when the Teflon sheet comes off, and when hands touch the shirt. So there are 3 fixes.
Step 1: press light (hot enough, long enough, but gentle)

- 175–180°C
- 50–60 seconds, or until the pretreatment is dry
- Lowest pressure possible: steam escapes easily, the pretreatment dries faster, and there are fewer pretreatment stains
- Pneumatic heat press: set 1–1.5 bar
- Manual lever press: close it gently, no force
These values sit inside the default range on the SK pretreatment product pages (heat press 165–180°C for 40–60 s).
Step 2: the Teflon sheet must not stick to the shirt

When you open the press, the Teflon sheet should come away from the shirt by itself, with no pulling or peeling. Then the fibres are not pulled up.

If the sheet sticks:
- Wipe the Teflon sheet with alcohol and a polyester cloth
- Press again for 5–10 seconds
- Check again: the sheet must lift off by itself
Step 3: load the shirt without touching the print area

When you put the shirt on the platen, do not touch the area you will print. If you need to straighten it, pull it by the corners. Touching makes the flattened fibres stand up again.
Small trick: mark the side that touches the shirt

Mark one side of the Teflon sheet as the shirt side and always put that side down. Dirt from the heat press then stays off the shirt, which helps a lot if the press is shared with other print jobs.
Easy to remember

- Press light: 175–180°C · 50–60 s · lowest pressure
- Sheet does not stick: lifts off by itself
- Do not touch the print: move the shirt by its corners
SK pretreatment
SK DTG pretreatment is made in Thailand in versions for each fabric and shirt colour: PRT-DTG-DC for dark cotton, PRT-DTG-UDC premium, PRT-DTG-WC for white and light shirts. See all at SK Pretreatment.
Still seeing fibres? Send a photo of the print to the SK team.
Written by the SK Color & Chemicals team from SK's own training video and SK pretreatment product pages · Updated Nov 2026
All drawings are simplified illustrations.